Lanthanum fluoride (LaF3) thin films were prepared by resistive heating evaporation and electron-beam gun evaporation under the same deposition rate, deposition substrate temperature, and vacuum pressure. The coated LaF3 films were then treated by heat annealing and UV light irradiation. The optical properties, microstructures, stress, and laser-induced damage threshold (LIDT) at a wavelength of 193 nm were investigated. The surface roughness, optical loss, stress, and LIDT of the films were improved after the annealing. The films had better properties when irradiated by UV light as compared with heat annealing.
© 2005 Optical Society of America
Full Article | PDF ArticleMore Like This
Cheng-Chung Lee, Ming-Chung Liu, Masaaki Kaneko, Kazuhide Nakahira, and Yuuichi Takano
Appl. Opt. 44(34) 7333-7338 (2005)
Ming-Chung Liu, Cheng-Chung Lee, Masaaki Kaneko, Kazuhide Nakahira, and Yuuichi Takano
Appl. Opt. 51(15) 2865-2869 (2012)
Ming-Chung Liu, Cheng-Chung Lee, Bo-Huei Liao, Masaaki Kaneko, Kazuhide Nakahira, and Yuuichi Takano
Appl. Opt. 47(13) C214-C218 (2008)